Anode materials calcination for lithium batteries: green petroleum coke (GPC coke), green needle coke, calcined petroleum coke (CPC coke), calcined needle coke, natural graphite and hard carbon.
| Parameter | Value |
|---|---|
| Capacity | 15 tons / day |
| Rated power consumption | 1954 kW |
| Maximum rated temperature of high-temperature section | 700 ℃ |
| Operating temperature of high-temperature section | 650 ℃ |
| High-temperature section temperature zone grouping | 6 Zone |
| Maximum rated temperature of high-temperature carbonization section | 1200 ℃ |
| Operating temperature of high-temperature carbonization section | 1150 ℃ |
| High-temperature carbonization section temperature zone grouping | 9 Zone |
| Oxygen content | ≤20 ppm |
| Cooling water consumption | 70-90 m³/h |
| Heating method | Electric heating |
| Equipment dimensions | 47.9×3.8×5.7m |